Junord cladding is made of good-quality Ostrobothnian fir, which is firm and sound-knotted.

Special attention is paid to surface quality of Junord-products. Junord cladding is also available end tongued and grooved, packaged or painted according to customer wishes. Junord cladding is used in the construction of the highest-quality detached houses in Finland.

 

Common infos

Profiles: UTV, UTK, UTW and wedge profile
Standard dimensions: thickness width effective width
UTV 20 mm 95/120 mm 85/110 mm
  22 mm 95/120/145/170 mm 85/110/135/160 mm
  28mm 145/170 mm 135/160 mm
UTK 22 mm 145 mm 135 mm
  28 mm 145 mm 135 mm
UTW 28 mm 170 mm  
Wedge profile 27 mm 146 mm  
  All other profiles, thicknesses and widths are available on special order.
Painting: Different standard colours for painting fir. Other colour shades are available on special order. The prime colour is environment-friendly and water-thin able.
Surface: It is processed with fine-sawing equipment for ideal appearance, durability and paint consumption.
Lengths: Sold in run-of-mill lengths from 2.4 to 5.4 m or, on special order, finger-jointed or cut into customer-specified lengths from 2 to 7.5 m.
Surface treatment: Products of heartwood, the heart side is towards the surface. End tonguing and grooving is available according to customer wishes.
Packaging: Shrink-wrapped or small-bundle packaging is available.
Special dimensions: Special dimensions, profiles, lengths and moisture contents are available according to customer wishes.

Dimensional drawings

» UTV drawing (pdf) » UTK drawing (pdf)
» UYK drawing (pdf) » UYL drawing (pdf)

Sustainable wood cladding

Sustainable wood cladding with long-term maintenance intervals is characterised by the following factors. – wood is hard heartwood of fir with a moisture content of 18% - the first surface treatment is carried out within 60 hours after the planning process. - The first treatment is done on all sides. - The paint is done by vacuum technology, which penetrates the protective substances in the wood grain inside. - The second surface treatment is carried out within two weeks after the first treatment. - After the treatments, removal of residual water stocks, making the surface smoother. - The third surface treatment is made on site, when the wood has adjusted to the final climatic conditions. (Preferably in spring).